Superior Corrosion Resistance, Specifically for Severe Sulfuric Acid Environments and High-End Chemical Equipment
| Element | C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Cu |
|---|---|---|---|---|---|---|---|---|---|
| Content % | 0.02 | 1 | 2 | 0.035 | 0.03 | 19.0–21.0 | 24.0–26.0 | 4.0–5.0 | 1.0–2.0 |
Density: 8.0 g/cm³
Melting Point: 1350–1400 °C
Thermal Conductivity: 12.9 W/(m·K)
Mechanical Properties: Tensile strength ≥490 MPa, elongation ≥35%
Thickness: 0.5–6.0 mm (tolerance ±0.07 mm)
Width: 1000 / 1219 mm
Surface: 2B (cold-rolled annealed), customizable electro-polished
Coil Weight: 3–8 t/coil, made-to-order

Coil Feeding into Processing Machine

Parallel Coil Processing Lines

Coil Thickness Measurement

Single Coil Packaging

Factory Coil Storage

Truck Loading of Coils
Use ERNiCrMo-3 welding wire; post-weld solution treatment required
Custom lead time 15–20 days, corrosion test report provided
Walmay will help match the right stainless product form and specification for your application, confirm quantities and packing needs, and provide requested documents based on order requirements.